Showing 25–36 of 48 results

  • DCP11

    DCP11

    DCP11/50

    $1,375.00

    View Product
    • Length 90/100
    • Width 35/35
    • Thickness 2/2
    • Resonant Frequency kHz (min, typ, max) 115, 150, 190/190, 255, 325
    • Force Constant (min, typ, max) 2.5, 5.5, 10/5.5, 11.5, 22.5
    • Tip Shape Conical
    • Coating Diamond Doped with Nitrogen
  • DCP10

    DCP10

    DCP10/15

    $483.00

    View Product
    • Length 100
    • Width 35
    • Thickness 2
    • Resonant Frequency kHz (min, typ, max) 190, 255, 325
    • Force Constant (min, typ, max) 5.5, 11.5, 22.5
    • Tip Shape Conical
    • Coating Diamond Doped with Nitrogen
  • PHA_NC

    PHA_NC

    PHA_NC/15

    PHA_NC/50

    Starting At $364.00

    View Product
    • Length 94/124
    • Width 34/34
    • Thickness 1.85/1.85
    • Resonant Frequency kHz 10.8, 12, 13.2/3.15, 3.5, 3.85
    • Force Constant 188, 235, 282/112, 140, 168
    • Tip Shape Cylindrical at the base, conic on the last 1000 nm
    • Coating Au Reflective
  • HA_FM/W₂C

    HA_FM/W₂C

    HA_FM/W₂C/15

    HA_FM/W₂C/50

    Starting At $330.00

    View Product
    • Length 223/183
    • Width 34/34
    • Thickness 3/3
    • Resonant Frequency kHz 69.3, 77, 84.7/103, 114, 125.4
    • Force Constant 2.8, 3.5, 4.2/4.8, 6, 7.2
    • Tip Shape Octahedral at the base, conic on the last 200 nm
    • Coating W₂C Conductive
  • HA_FM

    HA_FM

    HA_FM/15

    HA_FM/50

    Starting At $286.00

    View Product
    • Length 223/183
    • Width 34/34
    • Thickness 3/3
    • Resonant Frequency kHz 69.3, 77, 84.7/103, 114, 125.4
    • Force Constant 2.8, 3.5, 4.2/4.8, 6, 7.2
    • Tip Shape Octahedral at the base, conic on the last 200 nm
    • Coating Au Reflective
  • HA_HR_DCP

    HA_HR_DCP

    HA_HR_DCP/15

    HA_HR_DCP/50

    Starting At $500.00

    View Product
    • Length 93/123
    • Width 34/34
    • Thickness 3/3
    • Resonant Frequency kHz 387, 430, 473/225, 250, 275
    • Force Constant 24, 30, 36/12.8, 16, 19.2
    • Tip Shape Octahedral at the base, conic on the last 200 nm
    • Coating Doped Diamond
  • HA_HR/W₂C

    HA_HR/W₂C

    HA_HR/W₂C/15

    HA_HR/W₂C/50

    Starting At $330.00

    View Product
    • Length 93/123
    • Width 34/34
    • Thickness 3/3
    • Resonant Frequency kHz 342, 418, 480/207, 230, 253
    • Force Constant 27.2, 34, 40.8/13.6, 17, 20.4
    • Tip Shape Octahedral at the base, conic on the last 200 nm
    • Coating W₂C Conductive
  • HA_HR

    HA_HR

    HA_HR/15

    HA_HR/50

    Starting At $286.00

    View Product
    • Length 93/123
    • Width 34/34
    • Thickness 3/3
    • Resonant Frequency kHz 342, 418, 480/207, 230, 253
    • Force Constant 27.2, 34, 40.8/13.6, 17, 20.4
    • Tip Shape Octahedral at the base, conic on the last 200 nm
    • Coating Au Reflective
  • HA_NC/HAR

    HA_NC/HAR

    HA_NC/HAR/5

    Starting At $248.00

    View Product
    • Length 94/124
    • Width 34/34
    • Thickness 1.85/1.85
    • Resonant Frequency kHz 212, 235, 258.5/126, 140, 154
    • Force Constant 9.6, 12, 14.4/2.8, 3.5, 4.2
    • Tip Shape Octahedral at the base, conic on the last 200 nm
    • Coating Au Reflective
  • HA_NC/FD

    HA_NC/FD

    HA_NC/FD/10

    HA_NC/FD/30

    Starting At $670.00

    View Product
    • Length 94/124
    • Width 34/34
    • Thickness 1.85/1.85
    • Resonant Frequency kHz 212, 235, 258.5/126, 140, 154
    • Force Constant 9.6, 12, 14.4/2.8, 3.5, 4.2
    • Tip Shape Octahedral at the base, conic on the last 200 nm
    • Coating Au Reflective
  • HA_NC/W₂C

    HA_NC/W₂C

    HA_NC/W₂C/15

    HA_NC/W₂C/50

    Starting At $330.00

    View Product
    • Length 94/124
    • Width 34/34
    • Thickness 1.85/1.85
    • Resonant Frequency kHz 212, 235, 258.5/126, 140, 154
    • Force Constant 9.6, 12, 14.4/2.8, 3.5, 4.2
    • Tip Shape Octahedral at the base, conic on the last 200 nm
    • Coating W₂C Conductive
  • HA_NC

    HA_NC

    HA_NC/15

    HA_NC/50

    Starting At $286.00

    View Product
    • Length 94/124
    • Width 34/34
    • Thickness 1.85/1.85
    • Resonant Frequency kHz 212, 235, 258.5/126, 140, 154
    • Force Constant 9.6, 12, 14.4/2.8, 3.5, 4.2
    • Tip Shape Octahedral at the base, conic on the last 200 nm
    • Coating Au Reflective